Multiphysics modelling of Stress Corrosion Cracking by using peridynamics

D. De Meo, C Diyaroglu, N. Zhu, E. Oterkus, Muhammad Amir

Research output: Chapter in Book/Report/Conference proceedingChapter (peer-reviewed)

Original languageEnglish
Title of host publicationAnalysis and Design of Marine Structures V
EditorsCarlos Guedes Soares, R. Ajit Shenoi
PublisherCRC Press
Pages499-504
Number of pages6
ISBN (Electronic)978-1-315-68505-2
ISBN (Print)978-1-138-02789-3
Publication statusPublished - 2015

Cite this

De Meo, D., Diyaroglu, C., Zhu, N., Oterkus, E., & Amir, M. (2015). Multiphysics modelling of Stress Corrosion Cracking by using peridynamics. In C. Guedes Soares, & R. A. Shenoi (Eds.), Analysis and Design of Marine Structures V (pp. 499-504). CRC Press. https://www.crcpress.com/Analysis-and-Design-of-Marine-Structures-V/Guedes-Soares-Shenoi/9781138027893